Electrically Conductive Polymer Concrete Coatings

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Electrically Conductive Polymer Concrete Coatings

Author(s): J. J. Fontana

Publication: Symposium Paper

Volume: 99

Issue:

Appears on pages(s): 31-50

Keywords: bonding; bridge decks; cathodic protection; coatings; conductivity; corrosion; deterioration; electrical resistance; polymer concrete; substructures; vinyl resins; Materials Research

DOI: 10.14359/2369

Date: 5/1/1987

Abstract:
The corrosion of reinforcing steel embedded in concrete causes cracks and delamination in the concrete. The application of impressed current cathodic protection utilizing electrically conductive polymer concrete to distribute the current across concrete bridge deck surfaces is gradually becoming a standard practice in the highway industry. To protect the bridge substructures, a sprayable electrically conductive polymer concrete coating is being developed. This thin coating has a very low resistivity and can distribute the cathodic protection current across the concrete surfaces that are to be protected.