Title: Chemically Prestressed Precast Concrete Box Culverts

Author(s): Y. Tsuji and N. Miyake

Publication: Concrete International

Volume: 10

Issue: 5

Appears on pages(s): 76-82

Keywords: admixtures; chemically prestressed concrete; economics; tests; cracking (fracturing); crack width and spacing; culverts; precast concrete; expansive cement concretes; expansive cements; reinforced concrete;

DOI:

Date: 5/1/1988

Abstract:
Experiments on the use of expansive cement concrete to improve the mechanical behavior and lighten the weight of precast concrete box culverts are described. Results indicate that introducing chemical prestress to a box culvert allows a reduction in member thickness while maintaining acceptable cracking behavior.