Steel Reinforcing Bar Specifications in Old Structures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Steel Reinforcing Bar Specifications in Old Structures

Author(s): Gustav G. Erlemann

Publication: Concrete International

Volume: 21

Issue: 4

Appears on pages(s): 49-50

Keywords: deformation; reinforcing materials; reinforcing steels; strength; specifications

DOI:

Date: 4/1/1999

Abstract:
Rehabilitating sixty-year-plus aged reinforced concrete structures requires knowledge of the strength of the materials furnished during that era. Reinforcing bars manufactured during that period generally were Grade 33 (228 MPa) with various patented deformation patterns (ASTM A 15-11). During 1928 the U.S. Department of Commerce recommended standard bar sized, semi-standard deformations, and Grade 40 (276 MPa) minimum. In 1950, A 15 specified all reinforcing bars as round (#3 through #11) with A 305 deformation patterns. In 1964, A 408 added sizes #14S and #18S, and two strength levels: A 432 (Grade 60 - 414 MPa) and A 431 (Grade 75 - 517 MPa). Finally, during 1968, ASTM combined all previous reinforcing bar specifications into A 615.