Creep Studies of Polyester Polymer Concrete Under Flexural Loading

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Creep Studies of Polyester Polymer Concrete Under Flexural Loading

Author(s): N. Dharmarajan and C. D. Armeniades

Publication: Symposium Paper

Volume: 99

Issue:

Appears on pages(s): 17-30

Keywords: creep properties; flexural strength; polyester resins; strains; polymer concrete; stresses; temperature; Materials Research

DOI: 10.14359/2358

Date: 5/1/1987

Abstract:
The creep of unsaturated polyester/styrene polymer concrete (PC) under flexural loads was investigated using two PC systems with different resin contents, as well as the unfilled resin. Measurements were taken at temperatures, ranging from -5 to 60 C, time periods up to 160 hours, and stress levels from 4 to 12 MN/m², which represent stress-to-strength ratios of 0.3 to 0.7. The data obtained over these ranges of temperature, stress, and resin content were successfully superposed on a single master curve of creep compliance versus time. On the basis of these results, the authors propose a single expression that describes the creep compliance of the PC system as a product of separable functions of temperature, stress, resin content, and time