Measurement of Properties of Fiber Reinforced Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Measurement of Properties of Fiber Reinforced Concrete

Author(s): ACI Committee 544

Publication: Materials Journal

Volume: 85

Issue: 6

Appears on pages(s): 583-593

Keywords: abrasion tests; cavitation; compression tests; erosion; tests; cracking (fracturing); workability; creep properties; energy absorption; fatigue (materials); fiber reinforced concretes; flexural strength; freeze-thaw durability; impact tests; modulus of e

DOI: 10.14359/2355

Date: 11/1/1988

Abstract:
Laboratory and field experience in the testing of fiber reinforced concrete (FRC) has indicated the need to review existing test methods and to develop new methods where necessary to determine the properties of FRC. This report outlines procedures for specimen preparation in general and discusses testing, workability, flexural strength, toughness, and energy absorption. New test methods are suggested for impact strength and flexural toughness. The applicability of the following test methods to FRC are reviewed: air content, yield unit weight, compressive strength, splitting tensile strength, freeze-thaw, shrinkage, creep, modulus of elasticity, cavitation, erosion, and abrasion resistance.