A method for Predicting Sulfate Durability of Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: A method for Predicting Sulfate Durability of Concrete

Author(s): Carl D. Harmann and Edward Mangotich

Publication: Symposium Paper

Volume: 100

Issue:

Appears on pages(s): 2135-2152

Keywords: cements; chemical analysis; concrete durability; oxides; deterioration; fly ash; sulfate attack; sulfate resistance; tests; Materials Research

DOI: 10.14359/2339

Date: 4/1/1987

Abstract:
A laboratory study was conducted to evaluate the effect of replacement of up to 35 percent by weight of the design cement content in a concrete mix with Class C fly ash on sulfate durability characteristics. Seven trial batches, including a control, one Class F, and five Class C ash mixes, and three types of test specimens were used. The test sulfate environment consisted of immersion in a 10 percent pH regulated sodium sulfate solution for more than two years. Weekly measurements of weight change and expansion were used to evaluate sulfate durability. Analyses of the expansion data suggest a calculated chemical compositional relationship called the oxide durability factor may be useful in predicting sulfate durability.