Thin Sheet Glass and Synthetic Fabric Reinforced Concrete 60-120 lb pcf Density

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Thin Sheet Glass and Synthetic Fabric Reinforced Concrete 60-120 lb pcf Density

Author(s): Morris Schupack

Publication: Symposium Paper

Volume: 124

Issue:

Appears on pages(s): 421-436

Keywords: cellular concretes; concretes; density (mass/volume); fabric; fibers; glass fibers; mortars (material); reinforced concrete; reinforcing materials; synthetic fibers; Materials Research

DOI: 10.14359/2333

Date: 9/1/1990

Abstract:
The background to the development of two types of thin, fabric-reinforced, portland cement concrete sheets is described and range of properties given. Both normal weight and lightweight mortars (including cellular mortars) were used as a matrix. Glass or synthetic fiber continuous reinforcement in the form of fabric scrims and/or nonwoven three-dimensional fabric were used. The materials developed are potential substitutes for plywood, cement asbestos, and other types of sheet material that require the properties of weather resistance, incombustibility, nonbiodegradability, and economy. The test results also suggest that the matrix and reinforcement concepts developed will lead to applications in other reinforced concrete uses. The thin sheet materials lend themselves to easy manufacture in a comparatively simple plant.