Title: Automatic Adjustment of Concrete Mixtures

Author(s): K. W. Day

Publication: Concrete International

Volume: 12

Issue: 6

Appears on pages(s): 51-53

Keywords: admixtures; aggregate gradation; air entrainment; batching; concretes; mix proportioning; moisture content; quality control; setting (hardening); workability; Materials Research

DOI:

Date: 6/1/1990

Abstract:
Describes a system for automatic adjustment of concrete mix proportions that combines quality assurance with reactive quality control. The system integrates concrete and aggregate test data with batch proportion data to control strength, slump/workability, sandiness/cohesion, entrained air, and setting time.