Strength and Porosity ofHardened cement-Fly Ash Pastes in Hot Environment

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Strength and Porosity ofHardened cement-Fly Ash Pastes in Hot Environment

Author(s): M. N. Haque and O. A. Kayyali

Publication: Materials Journal

Volume: 86

Issue: 2

Appears on pages(s): 128-134

Keywords: cement pastes; fly ash; hardened paste structure; sorption; high temperature; porosity; strength; water; Materials Research

DOI: 10.14359/2274

Date: 3/1/1989

Abstract:
The effects of hot-dry (45 C, 20 percent relative humidity) and temperate (23 C, 40 percent relative humidity) exposure conditions on the strength development, pore-size distribution, water sorptivity, and hydroxyl ion concentration of the hydrated cement paste, with and without fly ash, were studied. Plain cement and fly ash-cement paste specimens of 0.30 water-cementitious materials ratio and 0.30 fly ash-total cementitious ratio were cast. The specimens were cured in a fog room for differing periods varying from 1 to 112 days before exposure to the two regimes. The results indicate that given adequate initial curing of 7 days, the strength and strength-development characteristics of the fly ash-cement paste system are superior to those of the plain cement paste in both hot-dry and temperate exposure conditions. Further, exposure to hot-dry environment increases the total porosity of both the cement and cement-fly ash paste specimens as compared to the companion continuously moist-cured specimens. The decreased water sorptivity of the fly ash-cement paste specimens after 7 days of initial fog curing is also indicative of the beneficial effects of fly ash usage in hot-weather conditions where strength and permeability characteristics of concrete are most important for its durability.