Use of Cementitious Materials Other Than Portland Cement

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Use of Cementitious Materials Other Than Portland Cement

Author(s): Alan D. Buck

Publication: Symposium Paper

Volume: 100

Issue:

Appears on pages(s): 1863-1882

Keywords: alkali-aggregate reactions; blast furnace slag; concretes, evaluation; expansion; fly ash; mortars (material); portland cements; silica; sulfate attack; tests; Materials Research

DOI: 10.14359/2263

Date: 4/1/1987

Abstract:
Different amounts of fly ash, silica fume, or ground granulated iron blast furnace slag have been used with portland cement in an effort to prevent excessive expansion due to alkali-silica reaction or sulfate attack or both. The test methods used to establish optimum proportions were ASTM C 441 and ASTM C 1012. Once the optimum proportions were known, concrete mixtures were made and tested.