Rehabilitation of a Weir, Sluiceway, and Canal Headworks

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Rehabilitation of a Weir, Sluiceway, and Canal Headworks

Author(s): Gary R. Mass; Charles C. Hutton; and Dinh Vu Bao

Publication: Concrete International

Volume: 21

Issue: 3

Appears on pages(s): 40-45

Keywords: damage; dams; roller compacted concrete; rehabilitation; spillway

DOI:

Date: 3/1/1999

Abstract:
This article presents the unique restoration of a river diversion structure critical to the agriculture of Vietnam. The construction and history of this concrete and masonry structure are described. Also described are the investigation of existing conditions, analysis of the structure, and unusual rehabilitation methods selected based on site and construction considerations.