Application of Styrene-Butadiene Latex Modified Portland Cement Concrete Overlays in Parking Structure repair and Rehabilitation

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Application of Styrene-Butadiene Latex Modified Portland Cement Concrete Overlays in Parking Structure repair and Rehabilitation

Author(s): Brian D. Irvin

Publication: Symposium Paper

Volume: 116

Issue:

Appears on pages(s): 1-14

Keywords: concrete slabs; latex (plastic); parking structures; reinforced concrete; renovating; repairs; styrene-butadiene resins; resurfacing; Materials Research

DOI: 10.14359/2249

Date: 8/1/1989

Abstract:
Styrene-butadiene latex modified concrete system is an effective technique for repair and rehabilitation of parking garage decks. The system appears to retard corrosion of the reinforcing steel and has many benefits, including ease of placement and workability, superior flexural and bonding strength, and deicer scaling resistance. Styrene-butadiene latex modified concrete can be applied in parking structures during the winter months with few problems.