Simulation of Uniform Bond Stress

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Simulation of Uniform Bond Stress

Author(s): Homayoun H. Abrishami and Denis Mitchell

Publication: Materials Journal

Volume: 89

Issue: 2

Appears on pages(s): 161-168

Keywords: bond (concrete to reinforcement); bonding; bond stress; coatings; epoxy resins; pullout tests; reinforcing steels; splitting tensile strength; strain; Materials Research

DOI: 10.14359/2237

Date: 3/1/1992

Abstract:
A new testing technique, which simulates uniform bond stress distribution along a reinforcing bar, is presented. This method enables the determination of the complete bond stress-versus slip response and enables the investigation of both pullout and splitting failures. Sample tests were performed to demonstrate the testing technique. This testing technique can be used to investigate the bond performance of reinforcing bars and prestressing strand and to study the influence of concrete strength and presence of epoxy coating.


ALSO AVAILABLE IN:

Electronic Materials Journal