Title: Protection Against Chloride-Induced Corrosion

Author(s): Neal S. Berke, DonaldD W. Pfeifer, and Thomas G. Weil

Publication: Concrete International

Volume: 10

Issue: 12

Appears on pages(s): 45-55

Keywords: calcium nitrate; chlorides; corrosion; economics; reviews; reinforced concrete; reinforcing steels; silica fume; Materials Research

DOI:

Date: 12/1/1988

Abstract:
Concrete structures are exposed to many severe environments. One of the most damaging is the corrosive action of external chlorides, found in deicing salts and saltwater marine environments. This article stresses the need for research to combat the serious and widespread problem of chloride-induced corrosion in concrete.