Pozzolanic Activity of Calcined Red Mud

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Pozzolanic Activity of Calcined Red Mud

Author(s): J. Pera and A. Sadr Momtazi

Publication: Symposium Paper

Volume: 132

Issue:

Appears on pages(s): 749-762

Keywords: amorphous phase; calcination; compressive strength; dehydration; durability; lime; metakaolin; mortars (material); pozzolanic reactions; red mud; temperature; Materials Research

DOI: 10.14359/2182

Date: 5/1/1992

Abstract:
Red mud is a by-product from the aluminum industry. To investigate the possibility of using this waste material as a pozzolan in the cement and concrete industries, tests were carried out to examine the pozzolanic properties of calcined red mud. Red mud was calcined for 5 hr at five different temperatures: 600, 650, 700, 750, and 800 C. Blended portland cements containing 30 or 50 percent of the calcined red mud were studied for hydration products, strength, and durability. The results indicated that the red mud had the maximum reactivity when calcined at 600 C, because on hydration the lime content of the blended cement was considerably reduced. The calcined red mud when used in combination with portland cement contributed to the formation of hydrated alumina-silicates and hydrogarnets. Very good compressive strengths were obtained with the blended cement containing 30 percent calcined red mud. Mortars cast with these blended cements were placed in solutions of seawater and acetic acid. The results indicated good stability of mortars to these environments.