ACI Defines High-Performance Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: ACI Defines High-Performance Concrete

Author(s): Henry G. Russell

Publication: Concrete International

Volume: 21

Issue: 2

Appears on pages(s): 56-57

Keywords: durability; high-performance concretes; specifications; strength criteria

DOI:

Date: 2/1/1999

Abstract:
Ever since the terminology "high-performance concrete" (HPC) was introduced into the industry, there have been numerous attempts to develop a definition. In 1998, the Technical Activities Committee and its subcommittee on high-performance concrete derived and approved an official ACI definition: "high-performance concrete – concrete meeting special combinations of performance and uniformity requirements that cannot always be achieved routinely using conventional constituents and normal mixing, placing, and curing practices." Commentary on the ACI definition is included.