Durability Properties of Overlays for Erosion-Damaged Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Durability Properties of Overlays for Erosion-Damaged Concrete

Author(s): Jahangir Mirza

Publication: Symposium Paper

Volume: 126

Issue:

Appears on pages(s): 279-294

Keywords: bonding; erosion; grouts; mortars (epoxy, polymer); permeability; thermal properties; thermal expansion; Materials Research

DOI: 10.14359/2169

Date: 8/1/1991

Abstract:
Erosion by abrasion, cavitation and/or chemical attack in concrete hydraulic structures deteriorates spillways, stilling basins, chutes, slabs and transverse joints, concrete blocks under water gates, and any irregular surface subjected to high water flow rate. Countless overlays are commercially available for repairing deteriorated surfaces. However, the essential data provided by manufacturers is very limited and, even if it is available, it is normally limited to room temperature values. This persuaded the Canadian Electrical Association to support a comprehensive study on commercial overlays, especially from the viewpoint of resistance against erosion and the severe climatic conditions observed in northern parts of Canada. This paper presents laboratory test data on the erosion resistance and durability properties of various types of commercial overlays such as cementitious grouts, polymer-modified cement-based mortars, and epoxy mortars.