Title: Simplified Version of the Recommended Practice for Evaluation of Strength Test Results

Author(s): ACI Committee 214

Publication: Materials Journal

Volume: 85

Issue: 4

Appears on pages(s): 272-279

Keywords: coefficient of variation; compression tests; concretes; compressive strength; concrete construction; cylinders; evaluation; quality control; sampling; standard deviation; statistical analysis; variations; Materials Research

DOI: 10.14359/2160

Date: 7/1/1988

Abstract:
The purpose of this report is to introduce the use of a simplified version of the statistical concepts as outlined in ACI 214 for the specification, control, and evaluation of the production of concrete. For a more elaborate discussion of the concepts, see the "Recommended Practice for the Evaluation of Strength Test Results of Concrete" (ACI 214).