Properties of Polyacrylonitrile Fiber Reinforced Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Properties of Polyacrylonitrile Fiber Reinforced Concrete

Author(s): H. Hahne, S. Karl, and J. D. Worner

Publication: Symposium Paper

Volume: 105

Issue:

Appears on pages(s): 211-224

Keywords: acrylic fibers; compressive strength; fiber reinforced concretes; flexural strength; polyacrylonitrile; pullout tests; shrinkage; Materials Research

DOI: 10.14359/2132

Date: 12/1/1987

Abstract:
In recent years, a high-tenacity acrylic fiber for technical applications was developed in West Germany. Test data using these special polyacrylonitrile fibers in mortar and concrete are presented. Within a limited parameter study, the amount and geometry of the fibers and the size of the largest aggregates of the matrix were varied. The produced specimens were tested concerning the flexural and compressive behavior as well as crack development due to shrinkage. To determine the optimal length of fibers, integral pullout tests were conducted. The modulus of rupture found in the experiments was used to show the effect of the fibers in a diagram that relates the size of the "plastic zone" to the critical crack width.