Shrinkage and Creep Behaviour of High Fly Ash Content Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Shrinkage and Creep Behaviour of High Fly Ash Content Concrete

Author(s): R. N. Swamy and H. B. Mahmud

Publication: Symposium Paper

Volume: 114

Issue:

Appears on pages(s): 453-476

Keywords: calcium; creep properties; concretes; fly ash; portland cements; shrinkage; stress-strain relationships; workability; Materials Research

DOI: 10.14359/2095

Date: 5/1/1989

Abstract:
Paper presents extensive test data on the shrinkage and creep behavior of high fly ash-content concrete made with ordinary portland cement and 50 percent by weight cement replacement with low-calcium Type F fly ash. The concrete mixes were designed to have 20, 40, and 60 MPa 28 day cube strength with high workability and low water-to-composite cement ratio. The other variables were the exposure condition for the shrinkage tests and stress-strength ratio for the creep tests. The results showed that for structural concrete of 40 to 60 MPa, the ultimate shrinkage strain ranged from 400 to 500 x 10-6 m/m. The swelling strain amounted to 40 to 55 percent of the shrinkage value and indicated the importance and continued water curing for effective realization of full pozzolanic action of the fly ash. For the same concrete strength of 40 to 60 MPa, the specific creep and the creep coefficient were remarkably low ranging from 40 to 100 x 10-6 /MPa and 1.20 to 2.50, respectively. The data clearly confirm that the time-dependent deformations of well-designed high fly ash-content concrete compare extremely well with those of portland cement concrete.