Where Did All That Air Come From?

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Where Did All That Air Come From?

Author(s): Carl Bimel

Publication: Concrete International

Volume: 21

Issue: 1

Appears on pages(s): 54-59

Keywords: air-entraining agents; air entrainment; durability; finishing; slab-on-ground construction

DOI:

Date: 1/1/1999

Abstract:
Second study from ACI Committee 302 (Construction of Concrete Floors) Finishing Task Force on air entrainment in slabs and subsequent delamination. Field study conducted in Phoenix, Arizona, provided data for this study. Author proposes reasons why air content is difficult to control under field conditions and why excessive air content is detrimental to slab finish and durability, especially when a smooth, hard troweled finish is specified for the slab on grade.




  

Edit Module Settings to define Page Content Reviewer