Title: Frost Lenses? Sure, but in Concrete?

Author(s): W. F. Perenchio, V. Kress, and D. Breitfeller

Publication: Concrete International

Volume: 12

Issue: 4

Appears on pages(s): 51-53

Keywords: concretes; freeze-thaw durability; freezing; ice formation; microcracking; setting (hardening); Materials Research

DOI:

Date: 4/1/1990

Abstract:
Describes the incidence of frost lenses in a warehouse floor slab that was subjected to freezing shortly after the concrete was placed. This phenomenon has not been reported in the literature since 1945.