Use of Pond Ash in CLSM

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Use of Pond Ash in CLSM

Author(s): Christine A. Langton, N. Rajendran, Stanley E. Smith

Publication: Concrete International

Volume: 20

Issue: 12

Appears on pages(s): 58-62

Keywords: field tests; low-strength materials; mix proportioning; pond ash

DOI:

Date: 12/1/1998

Abstract:
Mix proportions for Controlled Low Strength Material (CLSM) were developed that incorporate pond ashes (coal ash collected in ponds) from the A-Area, F-Area, and D-Area Ash Basins at the Savannah River Site, in Aiken, S. C. Laboratory and field test results indicate the three pond ashes can be incorporated into CLSM which meets all of the design specifications for the Savannah River Site. A mix proportion containing D-Area ash was formulated for use as structural fill. A CLSM mix was formulated for common fill applications using the A- and F-Area ashes, which were less homogenous than the D-Area ash and contain a larger amount of clinker and bottom ash.




  

Edit Module Settings to define Page Content Reviewer