Effect of Water-Cement Ratio and Curing on Chloride Penetration into Concrete Exposed to Mediterranean Sea Climate

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effect of Water-Cement Ratio and Curing on Chloride Penetration into Concrete Exposed to Mediterranean Sea Climate

Author(s): Chanoch Jaegermann

Publication: Materials Journal

Volume: 87

Issue: 4

Appears on pages(s): 333-339

Keywords: chlorides; concretes; corrosion; cover; curing; exposure; marine atmospheres; reinforcing steels; serviceability; water-cement ratio; Materials Research

DOI: 10.14359/2039

Date: 7/1/1990

Abstract:
The effect of water-cement ratio (w/c) and curing regime on chloride ion ingress of 20 x 20 x 12 cm specimens exposed to Mediterranean Sea climate was studied. Variants included: w/c of 0.4, 0.5, 0.6, and 0.75, and 1, 3, and 7 days of water curing at 30 C (86 F). Diffusion curves have been obtained from dry-drilled pulverized samples extracted in 5 mm (0.198 in.) steps after «, 1, 1 «, 2, and 3 years of exposure. A depth of 0.4 and 1.0 percent Cl threshold have been established for the different variants. A linear relationship was found between threshold depth and w/c ratio. The threshold values are linearly dependent on curing regime after 1 year of exposure. With time, dependence reduces. After 3 years' exposure, no significant dependence was observed. Explanations for results obtained are offered. Results are compared with local code requirements. Temporary recommendations include reduction of w/c ratio and increase of cover over reinforcing steel.