SP-257: FRP Stay-In-Place Forms for Concrete Structures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: SP-257: FRP Stay-In-Place Forms for Concrete Structures

Author(s): Editor: Amir Z. Fam / Sponsored by: ACI Committee 440

Publication: Symposium Paper

Volume: 257

Issue:

Appears on pages(s): 210

Keywords:

DOI: 10.14359/20258

Date: 11/1/2008

Abstract:
This CD-ROM consists of 11 papers which were presented in two special sessions sponsored by ACI Committee 440 at the ACI Spring Convention in Los Angeles, California, on March 31, 2008. The technical papers presented at the sessions and published in this volume cover both open and closed FRP forms, including bridge decks, concrete-filled tubes, and girders, and address important relevant aspects such as surface preparation, bond aspects, fatigue, constructability, confinement, and field applications.