SP-254: Nanotechnology of Concrete: Recent Developments and Future Perspectives

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: SP-254: Nanotechnology of Concrete: Recent Developments and Future Perspectives

Author(s): Editors: K. Sobolev and S.P. Shah / Sponsored by: ACI Committee 236

Publication: Symposium Paper

Volume: 254

Issue:

Appears on pages(s): 164

Keywords:

DOI: 10.14359/20092

Date: 10/1/2008

Abstract:
This volume consists of ten papers that were presented at a technical session, sponsored by ACI Committee 236, Materials of Science of Concrete, at the ACI Fall 2007 Convention in Denver, CO. Papers include “ Nanotechnology in Construction: A Roadmap for Development”, “ Nanotechnology and Concrete: Research Opportunities”, “Molecular Engineering of the Cohesion in Neat and Hybrid Cement Hydrates”, and “Use of Atomic Force Microscopy and Nanoindentation for Characterization of Cementitious Materials at the Nanoscale”.