Concrete Q & A: Minimizing Raveling at Saw Cut Joints

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Concrete Q & A: Minimizing Raveling at Saw Cut Joints

Author(s):

Publication: Concrete International

Volume: 30

Issue: 8

Appears on pages(s): 96

Keywords:

DOI:

Date: 8/1/2008

Abstract:
How can we prevent raveling at saw cut contraction joints? We recently saw cut a decorative concrete surface at the same time we normally do—the morning after placing the concrete—but the raveling still occurred.