Title: Long-Term Deflection of High-Strength Concrete Beams

Author(s): Kent A. Paulson, Arthur H. Nilson, and Kenneth C. Hover

Publication: Materials Journal

Volume: 88

Issue: 2

Appears on pages(s): 197-206

Keywords: beams (supports); compressive strength; creep properties; deflection; high-strength concretes; loads (forces); shrinkage; Materials Research

DOI: 10.14359/2008

Date: 3/1/1991

Abstract:
A large body of experimental evidence is now available to confirm that the creep coefficient of high-strength concrete under sustained axial compression is significantly less than that of ordinary concrete. Thus, the ratio of time-dependent deflection to immediate elastic deflection of high-strength concrete beams under sustained loads should also be lower. However, the long-term deflection multipliers of the 1989 ACI Building Code do not account for concrete strength as a variable. Experimental results are reported for nine beams with nominal concrete compressive strengths over a range to 12,000 psi, loaded over a 12-month period. These tests confirm the significant differences between beams using high-strength concrete and those using normal strength concrete. Based on these and other tests, modifications to the present ACI Building Code method of predicting long-term deflections are suggested.