Title: Waterproofing Below-Grade Shotcrete Walls

Author(s): Jason Darling and Xia Cao

Publication: Concrete International

Volume: 30

Issue: 11

Appears on pages(s): 50-52

Keywords: chemical grout; foundation; shotcrete; waterproofing

DOI:

Date: 11/1/2008

Abstract:
Preapplied waterproofing systems for below-grade foundation wall construction at confined sites have traditionally been designed for use with cast-in-place concrete. This can pose challenges for traditional waterproofing systems when shotcrete is selected. A new waterproofing system developed by Grace Construction Products and DeNeef Construction Chemicals uses proven chemical grout injection proactively to prevent water leaks before they occur.