Concrete Q & A: Calculating Development Length of Bundled Bars

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Concrete Q & A: Calculating Development Length of Bundled Bars

Author(s):

Publication: Concrete International

Volume: 27

Issue: 4

Appears on pages(s): 96

Keywords:

DOI:

Date: 4/1/2005

Abstract:
When calculating the development length of a group of bundled bars per ACI 318-05, Section 12.4.2 requires the equivalent bar diameter for the bundle to be used when determining the appropriate factors. What bar diameter is to be used when calculating the development length per Section 12.4.1?