Title: Mechanical Properties of High Performance Concrete

Author(s): Paul Zia, S. H. Ahmad, and M. L. Leming

Publication: Symposium Paper

Volume: 128

Issue:

Appears on pages(s): 543-558

Keywords: computer programs; high-strength concretes; highways; mechanical properties; research; Materials Research

DOI: 10.14359/2001

Date: 11/1/1991

Abstract:
Presents a discussion of the objectives, scope, and progress of a 4-year research project on the mechanical properties of high-performance concretes with particular reference to highway applications. High-performance concrete is defined by certain requirements of strength and durability.