309.1R-08: Report on Behavior of Fresh Concrete During Vibration

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 309.1R-08: Report on Behavior of Fresh Concrete During Vibration

Author(s): ACI Committee 309

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 18

Keywords: admixtures; aggregates; aggregate shape and texture; aggregate size; amplitude; compacting; consolidation; damping; energy; fresh concrete; hardening; history; mechanical impedance; mixture proportioning; reviews; rheological properties; stability

DOI:

Date: 8/1/2008

Abstract:
This report covers the rheological and mechanical processes that take place during consolidation of fresh concrete. The first chapter presents the historical developments relative to consolidating concrete. The second chapter provides notations and definitions. The third chapter deals with the rheological behavior of concrete during consolidation and the associated mechanisms of dynamic compaction. The fourth chapter presents the principles of vibratory motion occurring during vibration, vibratory methods, and experimental test results. Continuing research in the field of concrete vibration, as evidenced by the extensive literature devoted to the subject, is addressed.