Title: Flattooing Concrete Surfaces

Author(s): Tamryn Doolan and Edward Benus

Publication: Concrete International

Volume: 30

Issue: 8

Appears on pages(s): 48-51

Keywords: decorative concrete; etching; stain; stencil

DOI:

Date: 8/1/2008

Abstract:
A group of products developed by Surface Gel Tek, LLC, make cleaning and stenciling surfaces for decorative concrete safer, easier, and more environmentally friendly. Three of these products are combined in a process the company calls "FlattooingTM" - the art of tattooing images and graphics into concrete surfaces. Sample projects and a step-by-step walk through of the Flattooing process are presented.