Reducing Thermal and Autogenous Shrinkage Contributions to Early-Age Cracking

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Reducing Thermal and Autogenous Shrinkage Contributions to Early-Age Cracking

Author(s): Dale P. Bentz and Max A. Peltz

Publication: Materials Journal

Volume: 105

Issue: 4

Appears on pages(s): 414-420

Keywords: cracking; early ages; shrinkage

DOI: 10.14359/19904

Date: 7/1/2008

Abstract:
Early-age cracking continues to be a significant problem for new concrete construction. Two of the major contributors to such cracking are the heat released by cement hydration during the first few days of curing and the autogenous shrinkage that often occurs during the same time frame. In this paper, three potential alternatives for reducing these contributions by modifying the concrete mixture proportions are investigated, namely increasing the water-cement ratio (w/c), using a coarser cement, or replacing a portion of the portland cement with a coarse limestone powder. Each alternative reduces the heat generated per unit volume by either reducing the volumetric cement content or its early-age reactivity, and reduces autogenous shrinkage by increasing the interparticle spacing between grains in the three-dimensional microstructure. These reductions are quantified for paste and mortar systems by measuring their semi-adiabatic temperature rise and autogenous deformation along with measurements of compressive strength to indicate the strength trade-off that will be experienced in reducing the risk of early-age cracking. These mixtures each have the additional advantage that they should result in a cost savings in comparison with an initial (control) mixture.


ALSO AVAILABLE IN:

Electronic Materials Journal