301S-05: Specifications for Structural Concrete (Spanish)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 301S-05: Specifications for Structural Concrete (Spanish)

Author(s):

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 76

Keywords: acabado, acabado con agregados a la vista, acero de preesfuerzo, aire incorporado, aditivo, agregado, apuntalamiento, cemento, clima cálido, clima frío, colocación, concreto, concreto liviano, concreto arquitectónico.

DOI:

Date: 4/20/2005

Abstract:

Note: A newer version of this document exists. This document was replaced by 301S-10.

Estas especificaciones constituyen unas Especificaciones de Referencia que el profesional facultado para diseñar puede aplicar a cualquier proyecto de construcción, citándolas en las Especificaciones del mismo. El profesional de diseño registrado complementa los requisitos de estas especificaciones, según sea necesario, designando o especificando requisitos particulares del proyecto. El documento cubre materiales y dosificación del concreto; aceros de refuerzo y de preesfuerzo; producción, colocación, terminado y curado del concreto; y diseño y construcción de cimbras y encofrados. Se especifican también los métodos de tratamiento de juntas y elementos embebidos, reparación de defectos superficiales y acabados superficiales (construidos con encofrado y sin él).Se incluyen secciones separadas para el concreto arquitectónico, concreto liviano, concreto masivo, concreto preesforzado y concreto con compensación por retracción. Se incluyen también los requisitos para el ensayo, evaluación y aceptación del concreto, así como para la aceptación de estructuras.