Design and Analysis of Heavily Loaded Reinforced Concrete Link Beams for Burj Dubai

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Design and Analysis of Heavily Loaded Reinforced Concrete Link Beams for Burj Dubai

Author(s): Ho Jung Lee, Daniel A. Kuchma, William Baker, and Lawrence C. Novak

Publication: Structural Journal

Volume: 105

Issue: 4

Appears on pages(s): 451-459

Keywords: beam; design; nonlinear finite element analysis; reinforced concrete; shear; strut-and-tie model

DOI: 10.14359/19859

Date: 7/1/2008

Abstract:
This paper presents a study on the shear capacity and behavior of reinforced concrete link beams designed for the Burj Dubai Tower, which is the tallest building in the world and will be ready for occupancy in 2009. Several thousand reinforced concrete link beams were used in this structure to interconnect structural walls; in some cases, the factored shear forces in these link beams were up to three times the traditional nominal ACI shear force strength limit. This study presents an examination of the factors that control the design and behavior of heavily loaded reinforced concrete link beams. Nonlinear finite element analysis methods were used to validate and inform the design of the reinforced concrete link beams for Burj Dubai and to examine if the ACI nominal sectional shear force limit is appropriate for this type of member. The results illustrate the undue conservatism of the ACI design provisions and the role of nonlinear analyses in design.