Design of Deep Beams Using Strut-and-Tie Models--Part I: Evaluating U.S. Provisions

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Design of Deep Beams Using Strut-and-Tie Models--Part I: Evaluating U.S. Provisions

Author(s): Michael D. Brown and Oguzhan Bayrak

Publication: Structural Journal

Volume: 105

Issue: 4

Appears on pages(s): 395-404

Keywords: efficiency factor; strain energy; structural concrete; strut-andtie modeling

DOI: 10.14359/19853

Date: 7/1/2008

Abstract:
From published reports, a database of 596 tests of reinforced concrete beams with shear span-depth ratios less than 2 was assembled. That compilation of data was used to examine the strain energy in various truss models that could be used to model the test specimens. It was found that single direct strut between the load and one of the reaction points was the favored mechanism. The strut-and-tie modeling provisions of ACI 318-05 and AASHTO LRFD were evaluated using the results contained in the database. The results of the analysis indicate that the use of both ACI 318-05 and AASHTO LRFD does not produce levels of safety that meet a 5% exclusion limit.


ALSO AVAILABLE IN:

Electronic Structural Journal