330R-08: Guide for the Design and Construction of Concrete Parking Lots

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 330R-08: Guide for the Design and Construction of Concrete Parking Lots

Author(s): ACI Committee 330

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 36

Keywords: concrete pavement; curing; dowels; finishing; joints; load transfer; parking lot; subgrade; thickness; traffic loads.

DOI:

Date: 6/1/2008

Abstract:
Concrete parking lots serve many kinds of public facilities, commercial developments, businesses, and multifamily housing projects. They primarily accommodate parked vehicles, but may also provide maneuvering area sand access for delivery vehicles. The design and construction of concrete slabs for parking lots and outside storage areas share many similarities with the design and construction of streets and highways, but they also have some very distinct differences. A full appreciation of the difference sand the modification of design and construction procedures to take these differences into account can result in economical concrete parking lots that will provide satisfactory service for many years with little maintenance. This guide includes information on site investigation, thickness determination, design of joints and other details, durability considerations, paving operations, and quality-assurance procedures during construction. Maintenance and repair are also discussed.