Mechanical Properties of Hardened Cement Paste Exposed to Temperatures up to 700 C (1292 F)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Mechanical Properties of Hardened Cement Paste Exposed to Temperatures up to 700 C (1292 F)

Author(s): W. P. S. Dias, G. A. Khoury, and P. J. E. Sullivan

Publication: Materials Journal

Volume: 87

Issue: 2

Appears on pages(s): 160-166

Keywords: cement paste; compressive strength; concretes; fire resistance; hardened paste structure; high temperature; mechanical properties; microstructure; modulus of elasticity; Materials Research

DOI: 10.14359/1981

Date: 3/1/1990

Abstract:
Significant temperatures are identified in the range of 20 to 700 C (68 to 1292 F) for changes in strength and elastic modulus (both static and dynamic) of unsealed hardened cement paste, measured at the various temperatures as well as after cooling. These changes are correlated with chemical and microstructural changes reported in the literature. The beneficial effect, within limits, of thermal drying and loading on these mechanical properties are observed. It is concluded that these properties are dependent primarily on the maximum temperature of exposure, as opposed to the temperature at testing.