Title: BDSC: Binders for Durable & Sustainable Concrete

Author(s): Pierre-Claude Aitcin

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 500

Keywords:

DOI:

Date: 4/1/2008

Abstract:
Linking theory to practice, this book provides a better fundamental understanding of Portland cement and hydraulic binders which is necessary to make better concrete. In this rigorously presented work, Pierre-Claude Aitcin explains the complexity of the hydration reaction and how to make, use and cure durable and sustainable concrete. This book also details the problems with Portland cement composition at present and outlines the concept of an ideal hydraulic binder which is technically and ecologically efficient, as well as being long-lasting and robust. This book is a practical and innovative reference text which will be particularly relevant to engineers and chemists working in the Portland cement, concrete and admixture industries.


Product unavailable, please call +1.248.848.3800