Shear Strength of Thin-Webbed Post-Tensioned Beams

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Shear Strength of Thin-Webbed Post-Tensioned Beams

Author(s): Miguel Fernandez Ruiz and Aurelio Muttoni

Publication: Structural Journal

Volume: 105

Issue: 3

Appears on pages(s): 308-317

Keywords: bridge girder; concrete crushing; post-tensioning; shear strength; stress field; tendons; testing; web

DOI: 10.14359/19790

Date: 5/1/2008

Abstract:
This paper investigates the load-carrying mechanisms and the strength of thin-webbed, post-tensioned beams failing by crushing of the web. The shear strength in these members is significantly reduced because of the state of cracking in the web and because of the disturbance in the flow of stresses introduced by the prestressing tendons. The interaction between both effects is investigated. To that end, the results of six full-scale tests performed on actual prestressed beams extracted from a girder bridge are presented. The results are analyzed and various approaches for the modeling of such members are investigated and compared.


ALSO AVAILABLE IN:

Electronic Structural Journal