Title: The Hidden Meaning of Water-Cement Ratio

Author(s): Dale P. Bentz and Pierre-Claude Aitcin

Publication: Concrete International

Volume: 30

Issue: 5

Appears on pages(s): 51-54

Keywords: capillary stress; compressive strength; fineness; water-cement ratio

DOI:

Date: 5/1/2008

Abstract:
Concrete mixtures are almost always characterized by their water-cement ratio w/c. Unfortunately, the w/c is an abstract number without any particular meaning and is inversely related to concrete strength: the lower w/c, the greater the concrete compressive strength. As demonstrated in this article, the w/c also has a hidden meaning that helps explain its relationship to compressive strength and makes this relationship easier to understand.