Quantification of Effects of Fly Ash Type on Concrete Early-Age Cracking

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Quantification of Effects of Fly Ash Type on Concrete Early-Age Cracking

Author(s): Kyle A. Riding, Jonathan L. Poole, Anton K. Schindler, Maria C. G. Juenger, and Kevin J. Folliard

Publication: Materials Journal

Volume: 105

Issue: 2

Appears on pages(s): 149-155

Keywords: cracking; early-age creep; fly ash; mass concrete.

DOI: 10.14359/19755

Date: 3/1/2008

Abstract:
The mechanisms that contribute to early-age cracking are complex. Determining the relative importance of each mechanism as well as the combined cracking potential for a given concrete material is essential for the concrete industry to construct structures with a long service life. A method for quantifying the cracking risk of a concrete mixture is presented. The method involves testing for the concrete heat of hydration, setting time, free thermal and autogenous movement, restrained stress, and mechanical property development. The concrete uniaxial stress under restrained conditions is measured using a rigid cracking frame. This test setup was used to quantify the effects of using fly ash on the concrete cracking risk using four different fly ashes with varying calcium oxide contents. All fly ashes reduced the cracking risk because of the decrease in the heat of hydration of the cementitious materials and, to a lesser extent, the increased early-age creep.