Title: Extending the Service Life of Parking Structures

Author(s): K. Nam Shiu and Kyle Stanish

Publication: Concrete International

Volume: 30

Issue: 4

Appears on pages(s): 43-49

Keywords: durability; maintenance; parking garage; repair

DOI:

Date: 4/1/2008

Abstract:
Parking structures are subject to severe environments, but a well thought out plan can help owners efficiently manage the structure’s need for maintenance over the service life. The plan should be developed with an understanding of the importance of timely repair, identification of the root cause of deterioration, and repairs with an appropriate service life. Such a systematic approach will be useful for the restoration and maintenance of all structures.