Time-Dependent Analysis of Concrete Structures with Variable Structural System

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Time-Dependent Analysis of Concrete Structures with Variable Structural System

Author(s): Luigino Dezi and Angelo Marcello Tarantino

Publication: Materials Journal

Volume: 88

Issue: 3

Appears on pages(s): 320-321

Keywords: age; beams (supports); creep properties; loads (forces); mathematical models; moment distribution; segmental construction; structural analysis; structures; Materials Research

DOI: 10.14359/1970

Date: 5/1/1991

Abstract:
Graphs are presented for the immediate solution of the problem involving homogeneous viscoelastic structures with variable structural systems.