Title: Lateral Blow-out Failure of Headed Studs Near a Free Edge

Author(s): Furche, J. and Eligehausen, R.

Publication: Commentary Reference

Volume: D

Issue: 23

Appears on pages(s): pp. 235–252

Keywords:

DOI:

Date: 6/1/2005

Abstract:
Anchors in Concrete-Design and Behavior, ACI SP-130, American Concrete Institute, Detroit, Mich., 1991