Seismic Resistance of Reinforced Concrete Beam-Column Joints

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Seismic Resistance of Reinforced Concrete Beam-Column Joints

Author(s): Hanson, N. W., and Conner, H. W.

Publication: Commentary Reference

Volume: 11

Issue: 56

Appears on pages(s): pp. 533-560

Keywords:

DOI:

Date: 6/1/2005

Abstract:
Proceedings, ASCE, V. 93, ST5, Oct. 1967