Behavior of Fasteners Loaded in Tension in Cracked Reinforced Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Behavior of Fasteners Loaded in Tension in Cracked Reinforced Concrete

Author(s): Eligehausen, R., and Balogh, T.

Publication: Commentary Reference

Volume: D

Issue: 10

Appears on pages(s): pp. 365-379

Keywords:

DOI:

Date: 6/1/2005

Abstract:
ACI Structural Journal, V. 92, No. 3, May-June 1995