Tensile Strength and Diagonal Tension Resistance of Structural Lightweight Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Tensile Strength and Diagonal Tension Resistance of Structural Lightweight Concrete

Author(s): Hanson, J. A.

Publication: Commentary Reference

Volume: 11

Issue: 13

Appears on pages(s): pp. 1-40

Keywords:

DOI:

Date: 6/1/2005

Abstract:
ACI JOURNAL, Proceedings V. 58, No. 1, July 1961