Durability of High-Strength Concrete Containing a High-Range Water Reducer

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Durability of High-Strength Concrete Containing a High-Range Water Reducer

Author(s): Gary L. Robson

Publication: Symposium Paper

Volume: 100

Issue:

Appears on pages(s): 765-780

Keywords: admixtures; air entrainment; bridges (structures); tests; concrete durability; freeze-thaw durability; high-strength concretes; mix proportioning; water-reducing agents; Materials Research

DOI: 10.14359/1949

Date: 4/1/1987

Abstract:
Recent construction of a segmental, precast concrete cable-stayed bridge across the Ohio River at Huntington, W. Va., involved two specially designed concretes: one with 6000 psi minimum strength and one with 8000 psi minimum strength. Attaining these strength levels was markedly enhanced by the availability and use of high-range water reducers, even though the fear of non-durable concretes was also heightened. The contract for this bridge required that the contractor develop mix designs and conduct a field trial operation to "shake down" his production and placing process using these mix proportions. Tests of the concretes produced during this field trial indicated that air-entrained high-strength concretes containing HRWR easily met the minimum strength requirements, but would not withstand the freeze-thaw cycling of ASTM C 666. Paper discusses the efforts involved in developing suitable concrete proportions for this work and compares freeze-thaw durability of high-strength concretes with and without entrained air and with and without high-range water-reducing admixtures.